Wednesday, September 10, 2014

Mirror Coating Woes - Part 2

Picking up where I left off:
I took my mirror to the Community Center where the mirror coating machine is housed.  I met the gentlemen who would be performing the re-coating. As I mentioned the machine looks like something out of the 50's and 60's . They hooked up the air compressor and started warming up the unit.

While they were getting the machine ready a friend of mine began stripping off the old coating using an alkali solution. The center spot was the most stubborn part because of the glue.  Eventually the coating was stripped off and the glass was ready for coating.

The simple explanation on how this machine works is this.  The machine consists of a bell-shaped vacuum chamber, a tungsten filament upon which three small loops of aluminum (AL) are hung, and a small rectangular chamber, called a "boat", with a piece of Silicon Oxide (SO) about the size of a large sand grain.

The cleaned mirror is mounted in a metal frame with the surface to be coated facing down. The frame is placed on three metal posts. The AL and SO are now below the surface to be mirrored with a small movable mask in between. The bell vacuum chamber is evacuated as completely as possible.  This takes about 40 minutes.  Next, the mask is rotated out of the way remotely and the tungsten filament is heated white hot which vaporizes the aluminum which deposits on the surface of the glass mirror blank. The tungsten filament is then turned off and the boat is heated up.  Vaporized SO is then deposited on the mirrored surface where it combines with the aluminum to become a one molecule thick coating of SO2 (glass). The boat is then cooled, the chamber is pressurized and the glass blank is now a telescope mirror ready for use.

In the first attempt to coat my mirror the aluminum was deposited successfully but the SO boat was overheated which caused excessive SO to be deposited, which made the surface look like rainbows. We had time to make a second try so we cleaned the surface and tried it again.  Although the AL and SO were deposited OK the mask did not rotate out of way completely so there was a small arc of uncoated glass.  We had to call it quits for that night but the mirror was usable.

Three weeks later, after repairing the machine, we gave it a third try with successful results.  I now have a beautifully coated mirror and the images I see are breathtaking. I'm very pleased with my mirror now.  And the cost, a donation to the Community Center, was much less than I would have paid to have the mirror re-coated commercially.